Polliwog 2012: 2nd Coat

Friday morning I spent one and a half hours sanding the first coat of topside hull paint with 120 grit and applied the 2nd coat. Tomorrow I’ll sand the hull with 220 grit and apply the 3rd coat. Then later that same day remove the making from the transom and apply the 2nd coat of varnish it.